Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

NYCOA 5033 HST 33% Glass-Fiber Reinforced, Heat Stabilized, Translucent Nylon 66 Resin

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 30% Glass Fiber Filled
Manufacturer NYCOA, Inc.
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NYCOA 5033 HST 33% Glass-Fiber Reinforced, Heat Stabilized, Translucent Nylon 66 Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
NYCOA 5033 HST is a 33% glass fiber reinforced, heat stabilized, translucent Nylon 66 resin used for injection molding. It has been specifically formulated for see through storage tanks for automotive fluids. NYCOA 5033 HST has excellent chemical resistance to most greases, oils and other hydrocarbons, high thermal resistance and translucency. Typical automotive under the hood applications include reservoir bottles for brake oil, transmission fluid, engine coolant, and power steering fluid. It also finds application in fuel tanks for ATVs, lawn & garden equipment and handheld machines.Information provided by Nycoa, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Water Absorption 0.70 %
0.70 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ASTM D955
Linear Mold Shrinkage, Transverse 0.0080 cm/cm
0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 122
122
ASTM D785
Tensile Strength, Yield 200 MPa
29000 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Flexural Strength 260 MPa
37700 psi
ASTM D790
Flexural Modulus 8.90 GPa
1290 ksi
ASTM D790
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Izod Impact, Unnotched 10.0 J/cm
18.7 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 263 °C
505 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 260 °C
500 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 240 °C
464 °F
ASTM D648