ND Industries Vibra-Tite® Formula 3

Category Polymer , Adhesive , Thermoset
Manufacturer ND Industries, Inc
Trade Name Vibra-Tite®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ND Industries Vibra-Tite® Formula 3.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General DescriptionEngineered to be cost-effective and CFC-free, ND Vibra-Tite Formula 3 is a non-ozone depleting, locking and sealing coating for threaded fasteners. Vibra-Tite utilizes a special blend of acrylic resins to prevent fasteners from loosening-even under extreme vibration.Designed for use on male and female ApplicationsFrom tiny eyeglass screws to huge construction bolts, vibratite is ideal for use on fasteners of any size. In addition to supplying bottles and cans on Vibra-Tite for "User-Applied," on the job application, fasteners can be "Pre-Applied" at any of ND Industries eight regional service centers.Meets or exceeds military specification:Mis-28867U.S. Air Force Part # 19207U.S. Army Tank Automotive Command (General Dynamics) Part # 11663357National Stock Number NSN-8030-00-163-5792 OEM Standards:Detroit Diesel 9S244 & 9S256Grumman Aircraft Part # GF-105 CA1Allied Signal Aerospace Company Part # EMS73314
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 73.9 °C
165 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Descriptive Properties Value Comments
Chemical resistance to Salt Water Totally Resistant
Acts as a partial corrosion barrier
Chemical resistance to solvents Some Resistance
Chemical resistance to Water Totally Resistant
Color Red (Custom colors available)
Cured Form resilient plastic
Curing Mechanism Solvent Evaporation
Shelf Life indefinite
Solvent Methylethylketone