ND Industries 623 Heptane-Acetone SuperGlue accelerator

Category Other Engineering Material , Catalyst/Initiator , Polymer , Thermoset
Manufacturer ND Industries, Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ND Industries 623 Heptane-Acetone SuperGlue accelerator.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fast Acting SuperGlue accelerator, general purpose for porous surfaces or large gaps. Non-ozone depleting but flammable solvent
Physical Properties Metric English Comments
Viscosity 5.0 cP
5.0 cP
Processing Properties Metric English Comments
Cure Time >= 0.0500 min
>= 0.000833 hour
on metal (Fixture)
1440 min
24.0 hour
On metal (Full)
Descriptive Properties Value Comments
Color Clear