Multibase Multi-Flex® TPO D 6006 Grey

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO)
Manufacturer Multibase
Trade Name Multi-Flex® TPO
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPO D 6006 Grey.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by Multibase.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
ASTM D792-91
Linear Mold Shrinkage 0.013 cm/cm
0.013 in/in
ASTM D955-89
Melt Flow 1.2 g/10 min
1.2 g/10 min
(Condition L) ASTM D-1238-94a
Mechanical Properties Metric English Comments
Hardness, Shore D 59
59
10 sec; ASTM D-2240-95
Tensile Strength, Ultimate >= 3.62 MPa
>= 525 psi
ASTM D638-95
Elongation at Break >= 500 %
>= 500 %
ASTM D638-95
Tear Strength 19.0 kN/m
108 pli
ASTM D624-95