Multibase Multi-Flex® A 7802 TPE Blk Thermoplastic Elastomer

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer Multibase
Trade Name Multi-Flex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® A 7802 TPE Blk Thermoplastic Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM 792
Melt Flow 1.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 82
82
10 seconds; ASTM D2240
Tensile Strength, Yield 8.96 MPa
1300 psi
Elastic; ASTM D412
Elongation at Break 650 %
650 %
Elastic; ASTM D412
Flexural Modulus 0.0655 GPa
9.50 ksi
Method I (3 point load), Procedure B); ASTM D790
Tear Strength 43.8 kN/m
250 pli
ASTM D624
Thermal Properties Metric English Comments
Flammability, UL94 V-0
V-0
Users viewing this material also viewed the following: