Material Notes:
Note 1: The Durafoam™100% EPDM Series, Expanded Cellular Rubber Sheets, were tested for QUV Ultraviolet Light Exposure. Test specimens for each stock number were cut 3 inches by 11 inches from ¼ inch thick sheets. These test pieces were exposed for 120 hours to a cycle consisting of: 1. Light at 70°C for 8 hours 2. Dark at 50° C for 4 hours 3. Condensation Cooling for 15 minutesInformation provided by Monmouth Rubber & Plastics Corp.
Physical Properties Metric English Comments
Density 0.176 g/cc
0.00637 lb/in³
Water Absorption <= 1.0 %
<= 1.0 %
ASTM D1056
Linear Mold Shrinkage <= 0.017 cm/cm
<= 0.017 in/in
Note 1
Mechanical Properties Metric English Comments
Tensile Strength 0.483 MPa
70.0 psi
Elongation at Break >= 180 %
>= 180 %
Compressive Strength 0.0345 - 0.0621 MPa
5.00 - 9.00 psi
0.25
Descriptive Properties Value Comments
Color Grey
Users viewing this material also viewed the following: