Michelman® Michem® Lube 160PF Anionic carnauba wax emulsion

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Michem® Lube
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® Lube 160PF Anionic carnauba wax emulsion.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Anionic carnauba wax emulsionUsage: Michem® Lube 160PF is an APEO-free additive which imparts slip, abrasion resistance and anti-block properties, in a variety of coatings and varnishes.Compatible with ingredients used in many industries, including: Automotive care products; Building materials; Can and coil coatings; Concrete; Cordage and twine; Deck stains and sealants; Die lubricants; Fiber sizings; Floor polishes; Furniture coatings; Glass; Gloves, balloons, footwear and mechanical seals; Inks; Packaging films; Pressure-sensitive adhesives; Textiles; Urethane foam and VarnishesFood Contact Information when manufacuted in the USA: FDA:175.105: Components of adhesives. 175.300: Resinous and polymeric components of coatings.175.320: Resinous and polymeric components of coatings for polyolefin films. 176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted) 176.180: Components of paper and paperboard in contact with dry foods. When manufactured in Belgium product meets food contact regulations for: Germany: BfR Recommendation XIV and BfR Recommendation XXXVI (Restricted)Food Contact Information when manufactured in Belgium: FDA:175.105: Components of adhesives.Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.990 - 1.01 g/cc
0.990 - 1.01 g/cc
Volatiles 74.5 - 75.5 %
74.5 - 75.5 %
pH 4.5 - 7.0
4.5 - 7.0
1.0 - 12
1.0 - 12
Recommended pH of system
Brookfield Viscosity <= 15 cP
<= 15 cP
Spindle # 1, rpm 60
Descriptive Properties Value Comments
Appearance Cream colored, opaque liquid
Emulsifier Charge Anionic
Solids Type Carnauba