Michelman® Michem® In-Line Primer 30 Primer

Category Fluid , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Michelman®
Trade Name Michem® In-Line Primer
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Michelman® Michem® In-Line Primer 30 Primer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Primer for Digital PrintingUsage: Michem® In-Line Primer 030 imparts a print-receptive surface to paper substrates to improve the ink transfer and adhesion of HP Indigo Electroinks. It is used in the in-line priming unit available as options on both the WS6000 and WS6600 presses. The primer improves the surface of a wide range of paper substrates, both uncoated and clay-coated of various basis weights, as well as PSA label stocks with paper face-stocks, including textured papers.Application Data: Apply a drop to the surface. The colour will change from blue to yellow if the surface has acid functionality. Michem® In-Line Primer 030 is designed specifically for use in the in-line priming unit of an HP Indigo WS6600 printing press. As such, when run as instructed by HP Indigo on paper substrates, the ILP unit will apply the correct amount of primer to achieve optimal ink adhesion and press performance.When manufactured in Belgium product meets food contact regulations for: Europe: Euro. Res. AP(2004)1 (Restricted) and Commission Regulation (EU) n° 10/2011(Restricted) Germany: BfR Recommendation XIV (Restricted)and BfR Recommendation XXXVI (Restricted)Food Contact Information when manufactured in Belgium:FDA: 175.105: Components of adhesives. (Restricted) 175.300: Resinous and polymeric components of coatings. (Restricted) 175.320: Resinous and polymeric components of coatings for polyolefin films. (Restricted) 176.170: Components of paper and paperboard in contact with aqueous and fatty foods. (Restricted) 176.180: Components of paper and paperboard in contact with dry foods. (Restricted)Information provided by Michelman®
Physical Properties Metric English Comments
Specific Gravity 0.990 - 1.01 g/cc
0.990 - 1.01 g/cc
pH 8.0 - 10
8.0 - 10
Brookfield Viscosity <= 100 cP
<= 100 cP
Spindle # 1, rpm 60
Descriptive Properties Value Comments
Appearance White, translucent liquid