MetalTek J92240 14-4 PH® Precipitation Hardening Steel

Category Metal , Ferrous Metal , Stainless Steel , Cast Stainless Steel , Precipitation Hardening Stainless
Manufacturer MetalTek
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MetalTek J92240 14-4 PH® Precipitation Hardening Steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Produced under license of ARMCO Advanced Materials Corp. Information provided by MetalTek
Mechanical Properties Metric English Comments
Hardness, Brinell 286
286
Tensile Strength, Ultimate >= 1030 MPa
>= 149000 psi
Tensile Strength, Yield >= 895 MPa
>= 130000 psi
Elongation at Break >= 10 %
>= 10 %
Component Elements Properties Metric English Comments
Carbon, C <= 0.060 %
<= 0.060 %
Chromium, Cr 13.5 - 14.25 %
13.5 - 14.25 %
Copper, Cu 3.0 - 3.5 %
3.0 - 3.5 %
Iron, Fe 72.79 - 77.1 %
72.79 - 77.1 %
As Balance
Manganese, Mn <= 0.70 %
<= 0.70 %
Molybdenum, Mo 2.0 - 2.5 %
2.0 - 2.5 %
Nickel, Ni 3.75 - 4.75 %
3.75 - 4.75 %
Niobium, Nb (Columbium, Cb) 0.15 - 0.35 %
0.15 - 0.35 %
Nitrogen, N <= 0.050 %
<= 0.050 %
Silicon, Si 0.50 - 1.0 %
0.50 - 1.0 %
Tantalum, Ta <= 0.050 %
<= 0.050 %
Descriptive Properties Value Comments
Heat Treatment Homog, Solution, Age