Akzo Nobel Trigonox® C-40B-pd Peroxide Cure Agent

Category Other Engineering Material , Catalyst/Initiator , Polymer
Manufacturer Akzo Nobel
Trade Name Trigonox®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Akzo Nobel Trigonox® C-40B-pd Peroxide Cure Agent.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Trigonox C-40B-pd is a monofunctional peroxide which is used for the crosslinking of organic rubbers and silicone rubbers.Chemical Description: tert-Butyl peroxybenzoate, powder, 40% with inert fillersCAS Number: 614-45-9Acronym: TBPB; Tx CInformation provided by Akzo Nobel Polymer Chemicals.
Physical Properties Metric English Comments
One Hour Half Life Temperature 110 °C
230 °F
Storage Temperature <= 25.0 °C
<= 77.0 °F