Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Matrixx Group 85S7451 Flame Retardant 45% Glass Reinforced PET  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET) , Polyethylene Terephthalate (PET), 50% Glass Reinforced
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Matrixx Group 85S7451 Flame Retardant 45% Glass Reinforced PET  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Data provided by The Matrixx Group, formerly RePlas.
Physical Properties Metric English Comments
Specific Gravity 1.80 g/cc
1.80 g/cc
73°F; ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 152 MPa
22000 psi
0.125 in; ASTM D638
Flexural Modulus 12.4 GPa
1800 ksi
Tangent, 0.125 in; ASTM D790
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
0.125 in, 73°F; ASTM D256
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 75.0 °C
167 °F
Relative Thermal Index; UL746
Deflection Temperature at 0.46 MPa (66 psi) 238 °C
460 °F
0.125 in; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 204 °C
400 °F
0.125 in; ASTM D 648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
5VA

@Thickness 3.00 mm
5VA

@Thickness 0.118 in