Material Notes:
Master Bond UV15-7 is a one component, non-yellowing UV curable polymer system for high performance bonding, sealing, coating and encapsulation. Its most salient features include superior physical strength properties, low shrinkage upon curing and good non-yellowing stability. This system bonds well to a wide variety of similar and dissimilar substrates including glass, metals and plastics, such as polycarbonates, acrylics and a number of polyester films.
Physical Properties Metric English Comments
Viscosity 1400 - 1800 cP

@Temperature 23.0 °C
1400 - 1800 cP

@Temperature 73.4 °F
Mechanical Properties Metric English Comments
Hardness, Shore D 70
70
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 149 °C
300 °F
Minimum Service Temperature, Air -51.1 °C
-60.0 °F
Descriptive Properties Value Comments
Color Transparent