Malvern Minerals Trikup® PM Silane Treated Aluminum Hydroxide

Category Ceramic , Oxide , Aluminum Oxide , Other Engineering Material , Additive/Filler for Polymer
Manufacturer Malvern Minerals Company
Trade Name Trikup®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Malvern Minerals Trikup® PM Silane Treated Aluminum Hydroxide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Trikup® is a custom, silane treated alumina trihydrate or aluminum hydroxide. ATH is the largest volume flame retardant in the world. Trikup® adds additional functionality through the use of epoxy, amino, vinyl and other silanes chosen to react with specific resin systems. Trikup® contributes brightness, opacity, gloss and smoothness to coatings. Additionally, Trikup® is exceptional for arc track resistance in PCBs and other composites. Additional fields include high power bushings and insulators. Typical Applications: Coatings, Silicone Rubber, Plastics, Wire & Cable, Adhesives, SMC/BMC, CompositesInformation provided by Malvern Minerals Company.
Physical Properties Metric English Comments
Specific Gravity 2.42 g/cc
2.42 g/cc
Bulk Density 0.657 g/cc
0.0237 lb/in³
Brightness 93 %
93 %
GE Brightness
Oil Absorption 41 %
41 %
Moisture Absorption at Equilibrium 0.30 %
0.30 %
Free Moisture
Particle Size 9.0 - 11 µm
9.0 - 11 µm
Average
pH 9.0
9.0
Mechanical Properties Metric English Comments
Hardness, Mohs 2.5 - 3.5
2.5 - 3.5
Optical Properties Metric English Comments
Refractive Index 2.40
2.40
Component Elements Properties Metric English Comments
Al2O3 64.9 %
64.9 %
Fe2O3 0.0090 %
0.0090 %
Loss on Ignition(%) 34.6 %
34.6 %
Other 0.25 %
0.25 %
total soda
SiO2 0.010 %
0.010 %