MV Labs ZN100 Zn(OAC)2·xH2O Zinc acetate hydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs ZN100 Zn(OAC)2·xH2O Zinc acetate hydrate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 183.45 g/mol
183.45 g/mol
Descriptive Properties Value Comments
Assay 30% Zn
CAS Number 5970-45-6
Form White crystals
Purity 99.999%
Typical Impurities Cd = 4; Ca, Fe, Mg, Mn < 1 ppm