MV Labs EU500 EuF3 Europium(III) fluoride

Category Ceramic , Halide
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF MV Labs EU500 EuF3 Europium(III) fluoride.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 208.96 g/mol
208.96 g/mol
Descriptive Properties Value Comments
Assay 73% Eu
CAS Number 13765-25-8
Form White powder
Purity 99.99%
Typical Impurities Check with Manufacturer