Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

MV Labs CO1000 CoSO4·6H2O Cobalt(II) sulfate hydrate

Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF MV Labs CO1000 CoSO4·6H2O Cobalt(II) sulfate hydrate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 154.99 g/mol
154.99 g/mol
Descriptive Properties Value Comments
Assay 21% Co
CAS Number 60459-08-7
Form Red crystals
Purity 99.999%
Typical Impurities Na = 2; Fe, Ni, Si < 1 ppm