Category Ceramic
Manufacturer MV Laboratories
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF MV Labs CE300 Ce2(CO3)3·xH2O Cerium(III) carbonate hydrate.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information provided by MV Laboratories.
Physical Properties Metric English Comments
Molecular Weight 460.27 g/mol
460.27 g/mol
Descriptive Properties Value Comments
Assay 47% Ce
CAS Number 54451-25-1
Form Off-white powder
Purity 99.999%
Typical Impurities Rare Earths < 10 ND; Ca, Fe, Mg = 3 ppm