Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Zeon Chemicals Zetpol® 2030L Hydrogenated Nitrile Elastomomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Zeon Chemicals
Trade Name Zetpol®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Zeon Chemicals Zetpol® 2030L Hydrogenated Nitrile Elastomomer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Zetpol 2030L is a lower-Mooney version of a highly saturated copolymer of butadiene and acrylonitrile with high tensile strength, good heat resistance, good chemical resistance to aggressive fluids, and an excellent balance of properties over a wide variation of temperatures.HNBR with highest level of unsaturation available. Provides excellent dynamic properties. Especially suited for rolls and dynamic oil field components. FDA approved.
Physical Properties Metric English Comments
Specific Gravity 0.950 g/cc
0.950 g/cc
Iodine Absorption Number 51.8 - 61.4
51.8 - 61.4
mg/100mg; ZCI-T-004
Mooney Viscosity 50 - 65

@Temperature 100 °C
50 - 65

@Temperature 212 °F
(1+4); ZCI-T-003
Ash <= 0.50 %
<= 0.50 %
ZCI-T-005
Mechanical Properties Metric English Comments
Hardness, Shore A 67
67
ZCI-T-009
Tensile Strength at Break >= 9.797 MPa
>= 1421 psi
ZCI-T-008
Elongation at Break 300 %
300 %
ZCI-T-008
300% Modulus >= 0.00680 GPa
>= 0.986 ksi
ZCI-T-008
Descriptive Properties Value Comments
% HYD 85
Bound ACN (%, acrylonitrile) 34.9-37.5
Heat Loss (%) Max 0.5