LyondellBasell Pro-fax SR549M Polypropylene Random Copolymer, Clarified

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer LyondellBasell
Trade Name Pro-fax
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Pro-fax SR549M Polypropylene Random Copolymer, Clarified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Primary Processing Method: Injection Molding and Injection Stretch Blow MoldingKey Features: clarified polypropylene random copolymer resin, superior clarity, good impact and rigidity balance, good surface finish and color, low odor and low taste transfer, improved injection molding cycle timesApplications: containers, housewares, bottlesMeets FDA requirements in 21 CFR 177.1520 for all food contact applications up to 212°F (100°C).Description: Pro-fax SR549M clarified polypropylene random copolymer resin has good see-through and contact clarity in injection molding and injection stretch blow molding applications. This resin meets FDA requirements in the Code of Federal Regulations in 21 CFR 177.520 for all food contact, including cooking applications. All ingredients meet the chemical registration requirements of TSCA and DSL.Information provided by Montell Polyolefins.LyondellBasell is the successor company to Montell.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792B
Melt Flow 11 g/10 min

@Load 2.16 kg,
Temperature 230 °C
11 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 30.0 MPa
4350 psi
ASTM D638
Elongation at Yield 13 %
13 %
ASTM D638
Flexural Modulus 1.00 GPa
145 ksi
1% secant at 0.05 in/min; ASTM D790A
Izod Impact, Notched 0.660 J/cm
1.24 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 84.0 °C
183 °F
ASTM D648
Optical Properties Metric English Comments
Haze 10 %
10 %
ASTM D1003A