Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

LyondellBasell Plexar® PX5335 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE

Category Polymer , Thermoplastic , Polyethylene (PE) , Anhydride-Modified Polyethylene , LLDPE
Manufacturer LyondellBasell (former Equistar)
Trade Name Plexar®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LyondellBasell Plexar® PX5335 Extrudable Tie-Layer Resin, Anhydride Modified LLDPE.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Plexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and copolymers, such as EVA or EMA, polypropylene, polyamide (nylon), ethylene vinyl alcohol copolymers (EVOH), ionomer and other sealants, polyethylene terephthalate (PET) resins and copolymers, styrenic polymers, metal, paper and many others. Product grades tailored for blown and cast films, sheet and thermoforming, blow molding, extrusion coating and lamination, tubing, pipe, spray coating and other specialty applications are available in pellet form. Contact your Plexar sales and/or Equistar technical service representative for more information and specific recommendations for your application(s).Regulatory Status: PX5335 meets the requirements for the Food and Drug Administration regulation 21CFR 175.105 for adhesives. This regulation describes adhesives which may be safely used as components of articles intended for use in packaging, transporting or holding food in accordance with conditions outlined in that regulation. For an adhesive formulation to be used in compliance with Section 175.105, it must be used under conditions that prevent the material from becoming a component of food in more than insignificant, de minimis, amounts. For more information, please contact your Lyondell product safety representative. Processing Techniques: A process melt temperature above 410°F (210°C) is recommended to ensure adhesion between adherents. More specific suggestions can be made only when equipment, process parameters and conditions of use are known. Contact your Equistar Plexar technical service representative for more information.This product is from the former Equistar product line.
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ASTM D1505
Oxidative Induction Time (OIT) 118 min
118 min
ASTM D3895
Melt Flow 5.7 g/10 min
5.7 g/10 min
ASTM D1238
Thermal Properties Metric English Comments
Vicat Softening Point 99.0 °C
210 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature >= 210 °C
>= 410 °F