Buckeye Polymers BP RPP 3015 T NAT Polypropylene, Talc Filled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Talc Filler
Manufacturer Buckeye Polymers
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Buckeye Polymers BP RPP 3015 T NAT Polypropylene, Talc Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Information: Our Talc filled product lines exhibit excellent properties such as high stiffness, surface aesthetics, low coefficient of thermal expansion, low shrinkage, improved scratch and mar resistance, and resistance to some aggressive chemical agents. Buckeye Polymers can also customize these materials through the addition of UV packages, custom color matching, and processing additives.Product Features:Increased stiffness and heat deflectionGood UV resistanceIndustrial, appliance, construction marketsGood scratch and mar resistanceProcessing Method: Injection MoldingInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Melt Flow 15 - 21 g/10 min
15 - 21 g/10 min
ASTM D1238
Ash 28 - 32 %
28 - 32 %
ASTM D5630
Mechanical Properties Metric English Comments
Flexural Modulus >= 1.55 GPa
>= 225 ksi
ASTM D790
Izod Impact, Notched >= 0.641 J/cm
>= 1.20 ft-lb/in
ASTM D256