LyondellBasell Integrateâ„¢ NE542013 Functionalized Polyolefin

Category Polymer , Thermoplastic , Polyolefin
Manufacturer LyondellBasell (former Equistar)
Trade Name Integrate™
Port Shanghai port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF LyondellBasell Integrateâ„¢ NE542013 Functionalized Polyolefin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
INTEGRATE products are chemically modified polyolefins used to combine dissimilar materials for a variety of applications including molding articles, flexible materials and fiber technology or to provide property enhancements which fulfill final materials parameters. These products are particularly effective when the materials involved contain both polar and non-polar components. Specific ingredients may include polymers such as polyethylene and/or its copolymers, polypropylene and/or its copolymers, polyamides (nylons), polyacetates, cellulose, ionomers, polyethylene terephthalate (PET) resins and/or its copolymers as well as a variety of minerals, which can be used to improve strength or stiffness in the final composition. Individual product grades can be tailored for specific applications or properties. INTEGRATE products are available in pellet form. Contact your sales and/or Equistar technical service representative for more information and specific recommendations for your applications(s)
Physical Properties Metric English Comments
Density 0.943 g/cc
0.0341 lb/in³
ASTM D1505
Melt Flow 13 g/10 min
13 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 15.3 MPa
2220 psi
ASTM D638
Elongation at Break 650 %
650 %
ASTM D638
1% Secant Modulus 552 MPa
80000 psi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 106 °C
223 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 204 °C
400 °F