Material Notes:
Lucobit® combines the positive properties of polyolefins and bitumen. The material is black and consists of mixtures based on high quality polyethylene copolymers with varying additions of special and amorphous bitumen. Bitumen is integrated homogeneously in the polymer matrix and thus can be processed as free-flowing granules on conventional processing equipment.Lucobit® has proven to be a robust and reliable raw material for roofing and sealing membranes. Product provides improvements in:• corrosion protection • thermal insulation• weathering resistance • thermal stability• bonding and weldability • anti-static effect• filler acceptance • shrinkage reduction• environmental stress crack resistanceInformation provided by Lucobit AG
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
ISO 1183
Melt Flow 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore A 86
86
ISO 868
Modulus of Elasticity 0.0550 GPa
7.98 ksi
ISO 527
Thermal Properties Metric English Comments
Minimum Service Temperature, Air -25.0 °C
-13.0 °F
Low Temperature Flexural Test; DIN 53361
Processing Properties Metric English Comments
Processing Temperature 150 - 180 °C
302 - 356 °F
Profiles
160 - 230 °C
320 - 446 °F
Membranes
160 - 240 °C
320 - 464 °F
Coatings
Melt Temperature 160 - 220 °C
320 - 428 °F
Mold Temperature 10.0 - 40.0 °C
50.0 - 104 °F