Lucite International Elvacite ® 4104 Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Elvacite ®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Elvacite ® 4104 Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Elvacite® 4104 is designed for use in self-levelling flooring formulations, but can be used in a variety of coatings formulations, such as covercoats, heat seal lacquers and plastic coatings. It has excellent flexibility and good gloss. Additionally, it is compatible with a wide range of binders and waxes. Solutions of Elvacite® 4104 in methyl methacrylate monomer show unusually good viscosity stability, making this product an extremely good choice for Monomer/Polymer (MoPo) systems.Information provided by Lucite International
Physical Properties Metric English Comments
Viscosity Measurement 0.52 - 0.60
0.52 - 0.60
reduced viscosity (dl/g), 1 wt% in chloroform; Ubbelohde B Viscometer
Molecular Weight 135000 g/mol
135000 g/mol
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 40.0 °C
104 °F
Chemical Properties Metric English Comments
Total Acid Number 0.00
0.00