Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lucas-Milhaupt Ultra Flux Silver Brazing Flux

Category Metal , Nonferrous Metal , Solder/Braze Alloy
Manufacturer Lucas-Milhaupt
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucas-Milhaupt Ultra Flux Silver Brazing Flux.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Ultra Flux is a water base paste consisting of a unique combination of potassium salts of fluorine and boric acid. It is recommended for use with torch, induction, furnace, resistance, dip and other heating methods. Our quality control ensures a creamy consistency with no grittiness. It can be used in the concentrated or diluted form, be applied using a brush, dip or spray, and has excellent adhesion without cracking when applied to parts which are air dried or heat dried before brazing.Information provided by Lucas-Milhaupt Warwick, LLC (formerly Wolverine Joining Technologies).
Physical Properties Metric English Comments
Water Absorption <= 35 %
<= 35 %
pH 8.0
8.0
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 871 °C
1600 °F
Minimum Service Temperature, Air 593 °C
1100 °F
Descriptive Properties Value Comments
Composition Potassium salts of fluorine and boric acid
Dilution Water (60cc/lb)
Heat 150-170F
Type Paste - Particle size #325 mesh or finer