Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Lubrizol ESTANE® 54660 Ester Based Thermoplastic Polyurethane (European Grade)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyurethane, TP , Thermoplastic Polyurethane, Elastomer, Polyester Grade
Manufacturer Lubrizol (former Noveon)
Trade Name ESTANE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lubrizol ESTANE® 54660 Ester Based Thermoplastic Polyurethane (European Grade).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability in a flexible thermoplastic elastomer system that is easy to process in a wide range of equipment. The Estane® TPU portfolio of products offers high performance polyester - and polyether - based resins and compounds in a broad range of hardnesses to meet a variety of application needs.Benefits of Estane® TPU: Outstanding Abrasion and Wear ResistanceExcellent Low Temperature FlexibilitySuperior Toughness and DurabilityEase of Processing and Manufacturing FlexibilityColorability and Paintability with no adhesion promoterApplications: Film & SheetFabric coating & melt coatingWire & CableHose, Tube & ProfileCustom moldingCustom compoundingAutomotive interior/chassis and exterior painted trimInformation provided by Noveon, Inc.
Physical Properties Metric English Comments
Specific Gravity 1.19 g/cc
1.19 g/cc
DIN 53479
Mechanical Properties Metric English Comments
Hardness, Shore A 76
76
DIN 53505
Tensile Strength, Ultimate 23.0 MPa
3340 psi
DIN 53504
Elongation at Break 840 %
840 %
DIN 53504
50% Modulus 0.00150 GPa
0.218 ksi
DIN 53504
100% Modulus 0.00190 GPa
0.276 ksi
DIN 53504
300% Modulus 0.00340 GPa
0.493 ksi
DIN 53504
Tear Strength 40.0 kN/m
228 pli
DIN 53515
Abrasion 25
25
mm<sup>3</sup>; DIN 53516
Thermal Properties Metric English Comments
Brittleness Temperature -70.0 °C
-94.0 °F
DIN 53546
Copyright © lookpolymers.com All Rights Reserved