Lord Adhesives Chemlok® 608 Adhesive

Category Polymer , Adhesive
Manufacturer Lord Adhesives
Trade Name Chemlok®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lord Adhesives Chemlok® 608 Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LORD Chemlok® 608 adhesive is a one-coat adhesive designed for bonding unvulcanized silicone elastomers to various rigid substrates.Chemlok 608 adhesive also provides excellent adhesion to a wide variety of commercially available silicone compounds which require a post cure.All information provided by Lord.
Physical Properties Metric English Comments
Density 0.8388 g/cc
0.03030 lb/in³
Solids Content 18 - 21 %
18 - 21 %
Thermal Properties Metric English Comments
Flash Point 3.00 °C
37.4 °F
Seta
Processing Properties Metric English Comments
Shelf Life 24.0 Month

@Temperature 21.0 - 27.0 °C
24.0 Month

@Temperature 69.8 - 80.6 °F
Descriptive Properties Value Comments
Appearance Clear to Hazy Pale Yellow Liquid
Solvents Methanol, Ethanol, Naphtha, Isopropanol