Loctite® PRISM® 411 Clear Instant Adhesive

Category Polymer , Adhesive , Thermoset , Acrylic/Cyanoacrylate Adhesive
Manufacturer Loctite
Trade Name PRISM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Loctite® PRISM® 411 Clear Instant Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Cyanoacrylate Bonding AdhesivesLoctite® technology has made the productivity promises of cyanoacrylate adhesives a reality with the industry's widest selection of high-performance, application-specific, instant adhesives. Loctite® Instant Adhesives are available in a variety of viscosities, cure speeds, gap-filling capability and substrate compatibility. The ultra high-performance PRISM® family offers additional products that surpass the most stringent demands, including toughened formulations, low odor and low blooming products, surface insensitive and thermally resistant formulations.Loctite® 411 Toughened Ethyl PRISM® Clear Instant AdhesiveAn adhesive formulated for excellent impact and peel strength in gap-filling applications. Cure Type: 7387 Bonding Type: Cyanoacrylate Typical Use: Clear gap filling.
Physical Properties Metric English Comments
Density 1.07 g/cc
0.0387 lb/in³
Viscosity 5000 cP
5000 cP
Mechanical Properties Metric English Comments
Adhesive Bond Strength 22.1 MPa
3200 psi
Grit blasted steel
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 98.9 °C
210 °F
Minimum Service Temperature, Air -53.9 °C
-65.0 °F
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified
Processing Properties Metric English Comments
Cure Time 0.500 min
0.00833 hour
1440 min
24.0 hour
Full Cure; Varies with substrates
Descriptive Properties Value Comments
Color Clear
Gap Fill 0.008 in.