Dow Corning SILASTIC® LSR 9151-200P PARTS A&B

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name SILASTIC®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning SILASTIC® LSR 9151-200P PARTS A&B.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A solventless, 2-part liquid silicone rubber available in white which has excellent water and chemical resistance, low and high temperature stability from -60 to 200 C (-76 to 392 F) and rapid cure at elevated temperatures.Information provided by Dow Corning
Physical Properties Metric English Comments
Viscosity 13000 cP
13000 cP
dynamic
Mechanical Properties Metric English Comments
Hardness, Shore A 39
39
Tensile Strength, Ultimate 1.38 MPa
200 psi
Elongation at Break 180 %
180 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 200 °C
392 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Processing Properties Metric English Comments
Pot Life 1440 min
1440 min
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Color white
Mix Ratio (X:1) 10
Base to Catalyst
Water Resistant yes