Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Latrobe Lescalloy® HY-180 VIM-VAR ; .375 - 2 thickness High Strength Alloy Steel

Category Metal , Ferrous Metal , Alloy Steel , Carbon Steel , Medium Carbon Steel
Manufacturer Latrobe Steel
Trade Name Lescalloy®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Latrobe Lescalloy® HY-180 VIM-VAR ; .375 - 2 thickness High Strength Alloy Steel.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
LESCALLOY HY-180 VIM-VAR steel is a high strength alloy steel with superior toughness. It is double vacuum melted (VIM-VAR…vacuum induction melted followed by vacuum arc remelting) to provide superior cleanliness and ingot homogeneity, and to enhance mechanical properties.Mechanical Properties from FMS-1111 SpecificationInformation Provided by Timken Latrobe Steel.Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.
Physical Properties Metric English Comments
Density 7.75 g/cc
0.280 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1310 MPa
190000 psi
Tensile Strength, Yield 1241 MPa
180000 psi
Elongation at Break 15 %
15 %
Reduction of Area 65 %
65 %
Modulus of Elasticity 190 GPa
27600 ksi
Charpy Impact 81.0 J

@Temperature -17.8 °C
59.7 ft-lb

@Temperature 0.000 °F
V-notch
Component Elements Properties Metric English Comments
Carbon, C 0.13 %
0.13 %
Chromium, Cr 2.0 %
2.0 %
Cobalt, Co 8.0 %
8.0 %
Iron, Fe 78.72 %
78.72 %
Manganese, Mn 0.10 %
0.10 %
Molybdenum, Mo 1.0 %
1.0 %
Nickel, Ni 10 %
10 %
Silicon, Si 0.050 %
0.050 %
Chemical Properties Metric English Comments
Critical Temperature 166 °C
331 °F
Mf
327 °C
621 °F
Ms
624 °C
1160 °F
Ac1
793 °C
1460 °F
Ac3
Users viewing this material also viewed the following: