LG Chemical HYPERIER IP1106 PA-PE Nanoclay Compound

Category Polymer , Thermoplastic , Nylon , Polyethylene (PE)
Manufacturer LG Chemical
Trade Name HYPERIER
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF LG Chemical HYPERIER IP1106 PA-PE Nanoclay Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
HYPERIER is a nano compound made from nano-sized inorganic plate clay. Excellent Barrier Performance, High StiffnessApplication: 1L~10L: Agrochemical Container, SORE Fuel Tank, PFCCAS No. 25750-23-6 and 9002-88-4Information provided by LG Chemical
Physical Properties Metric English Comments
Specific Gravity 1.03 g/cc
1.03 g/cc
Thermal Properties Metric English Comments
Melting Point 220 - 230 °C
428 - 446 °F