KiON CERASET® POLYSILAZANE 20 (PSZ 20)

Category Fluid , Polymer , Thermoset
Manufacturer KiON, A Clariant Business
Trade Name CERASET®
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF KiON CERASET® POLYSILAZANE 20 (PSZ 20).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
General DescriptionKiON Ceraset Polysilazane 20 is a liquid polymer that can easily be converted to a solid pre-ceramic and then be pyrolyzed to either silicon carbide or silicon nitride-containing ceramics.ApplicationsCeramic Matrix Composites (CMC’s), Metal Matrix Composites (MMC’s), ceramic slurry casting, ceramic and metal adhesives, and SiC/Si3N4 coatings for C/C, C/SiC, or SiC/SiC composites and ceramic nanocomposites.Information provided by KiON, A Clariant Business.
Physical Properties Metric English Comments
Density 1.02 g/cc
0.0368 lb/in³
Liquid
1.12 g/cc
0.0405 lb/in³
Cured Solid
2.40 g/cc
0.0867 lb/in³
Ceramic
Viscosity 184 - 200 cP

@Temperature 19.0 °C
184 - 200 cP

@Temperature 66.2 °F
Descriptive Properties Value Comments
%Resin 100% solids as liquid
Appearance Clear to pale yellow