Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Kennametal Stellite Stellite® 694 Cobalt Alloy

Category Metal , Nonferrous Metal , Cobalt Alloy , Superalloy
Manufacturer Kennametal Stellite
Trade Name Stellite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Kennametal Stellite Stellite® 694 Cobalt Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Kennametal Stellite'sâ„¢ cobalt base alloys are available as cobalt rods, cobalt electrodes, cobalt wire and cobalt powder.Cobalt alloys are used primarily for wear applications and are particularly well-suited for hardfacing applications.Information provided by Kennametal Stelliteâ„¢
Component Elements Properties Metric English Comments
Carbon, C 0.90 %
0.90 %
Chromium, Cr 28.5 %
28.5 %
Cobalt, Co >= 41.1 %
>= 41.1 %
as balance
Iron, Fe <= 3.0 %
<= 3.0 %
Nickel, Ni 5.0 %
5.0 %
Silicon, Si <= 1.0 %
<= 1.0 %
Tungsten, W 19.5 %
19.5 %
Vanadium, V 1.0 %
1.0 %
Descriptive Properties Value Comments
Application Technique PTA & laser deposition
Users viewing this material also viewed the following: