Production Method: P2ES-12 is produced from low density polyethylene, modified by carbon black, rubber and calcium stearate. Application: Designed for production of pipes used for explosive material, as well as for production of carpets and table cloths where the absence of static electricity charges is necessary.Information Provided by Kazanorgsintez
Physical Properties Metric English Comments
Volatiles <= 0.10 %
<= 0.10 %
Carbon Black Loading >= 18.5 %
>= 18.5 %
Melt Flow 0.10 - 1.0 g/10 min
0.10 - 1.0 g/10 min
Mechanical Properties Metric English Comments
Elongation at Break >= 145 %
>= 145 %
Tear Strength Test >= 9.5
>= 9.5
MPa
Electrical Properties Metric English Comments
Volume Resistivity <= 1000 ohm-cm
<= 1000 ohm-cm
Descriptive Properties Value Comments
Appearance Black pellets. Their size in any direction has to be 1.4 to 5 mm.