Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Karina E 890-25/1-CR-IS Natural PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Karina E 890-25/1-CR-IS Natural PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Flame retardant and oil resistant PVC compound, recommended for thin wall insulation of automotive electrical wires for working at the temperature range of -40°C to 105°C.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.39 - 1.45 g/cc
1.39 - 1.45 g/cc
ASTM D 792
ASTM Color 6.76 - 9.76
6.76 - 9.76
Color A, ME 12
86.8 - 89.8
86.8 - 89.8
Color L, ME 12
Mechanical Properties Metric English Comments
Hardness, Shore A 87 - 91

@Time 15.0 sec
87 - 91

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 14.7 MPa
>= 2130 psi
ASTM D 638
Elongation at Break >= 250 %
>= 250 %
ASTM D 638
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 105 °C
221 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Oxygen Index >= 26 %
>= 26 %
NBR 6245
Electrical Properties Metric English Comments
Volume Resistivity >= 3.00e+13 ohm-cm
>= 3.00e+13 ohm-cm
ASTM D 257
Descriptive Properties Value Comments
Application -40 Grades/+105 Grades
Users viewing this material also viewed the following: