Karina E 70/236-D-IS Clear PVC Compound

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Flexible Grade , PVC, Sheet Grade
Manufacturer Karina Indústria e Comércio de Plásticos
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Karina E 70/236-D-IS Clear PVC Compound.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
PVC compound recommended for freezer hanging screens extrusion.Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Physical Properties Metric English Comments
Specific Gravity 1.20 - 1.26 g/cc
1.20 - 1.26 g/cc
ASTM D 792
Mechanical Properties Metric English Comments
Hardness, Shore A 73 - 77

@Time 15.0 sec
73 - 77

@Time 0.00417 hour
ASTM D 2240
Tensile Strength >= 13.7 MPa
>= 1990 psi
ASTM D 638
Elongation at Break >= 250 %
>= 250 %
ASTM D 638
Descriptive Properties Value Comments
Application Flexible Sheet
Clarity OK
ME 03