Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

KKPC KOSYN KTR 401 Thermoplastic Elastomer (TPE)

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Korea Kumho Petrochemical Co., Ltd.
Trade Name KOSYN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KKPC KOSYN KTR 401 Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Thermoplastic Elastomer (TPE)Characteristics: KOSYN KTR101 is linear block copolymer made by solution polymerization which polymerizes butadiene and styrene in organic solvent. It is thermoplastics free of vulcanization and has superior tensile strength and elasticity.Applications: Asphalt roofing, waterproof agent, modifier and adhesives.Additional Notes: Bound Styrene: 30%Volatile Matter: 0.5%; ASTM D1416Ash Content: 0.15%; ASTM D1416This product is so sensitive to sunlight and humidity that it can be tarnished and caused deterioration of quality if exposed. It is recommended to store it in cool and shady area lest it should be exposed to direct sunlight. Do not expose to incompatible materials or contaminants.Data provided by Korea Kumho Petrochemical Co., Ltd.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ISO 2781
Brookfield Viscosity 22.76 cP
22.76 cP
25% by weight in toluene; ASTM D445
Melt Flow <= 1.0 g/10 min

@Load 5.00 kg,
Temperature 200 °C
<= 1.0 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
5 sec; ASTM D2240
Tensile Strength, Ultimate 16.0 MPa
2320 psi
ASTM D412
Elongation at Break 680 %
680 %
ASTM D412
Modulus of Elasticity 0.0280 GPa
4.06 ksi
ASTM D412