KKPC KOSYN KBR 710L Polybutadiene Rubber (Low cis BR)

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE)
Manufacturer Korea Kumho Petrochemical Co., Ltd.
Trade Name KOSYN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KKPC KOSYN KBR 710L Polybutadiene Rubber (Low cis BR).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Polybutadiene Rubber (Low cis BR)Characteristics: Low cis BR is different in cis content according to the production process and the catalyst. KKPC's low cis LBR has 35% cis content. LBR has high elasticity and reactivity containing about 14% vinyl bond structure. It is used in the tires of motorcycle, footwear, common industrial products, and also utilized as base polymer of HIPS (high impact polystyrene) which is widely used in cabinet of home appliances, interior decoration, and toys. Since these products have high Mooney viscosity and low solution viscosity, it's easier to control rubber particle size and reduce power consumption during processing. Applications: Footwear, HIPS products, mechanical productsAdditional Notes: cis-1,4 Contents: 34.5%Volatile Matter: 0.5%Ash Content: 0.01%Toluene insoluble gel: 0.01%Gel Rank: AThis product is so sensitive to sunlight and humidity that it can be tarnished and caused deterioration of quality if exposed. It is recommended to store it in cool and shady area lest it should be exposed to direct sunlight. Do not expose to incompatible materials or contaminants.Data provided by Korea Kumho Petrochemical Co., Ltd.
Physical Properties Metric English Comments
Viscosity 90 cP
90 cP
Viscosity of Solution; 5% Styrene
Mooney Viscosity 32

@Temperature 100 °C
32

@Temperature 212 °F
ML1+4
Descriptive Properties Value Comments
Color 7
APHA