KB Alloys 15% Strontium Aluminum Alloy

Category Metal , Nonferrous Metal , Aluminum Alloy
Manufacturer KB Alloys
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF KB Alloys 15% Strontium Aluminum Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
With the use of master alloys containing special addition agents, many characteristics can be imparted to aluminum alloys. Master alloys containing beryllium are added to aluminum magnesium melts at low levels to reduce magnesium losses. Small beryllium additions also improve surface quality of DC billet as well as impart improved mechanical properties to premium quality aluminum casting. The electrical and thermal conductivity of aluminum can be improved by the addition of trace amounts of boron to eliminate the undesirable effects of chromium, titanium, vanadium and zirconium. Boron also provides an effective grain refiner for aluminum silicon alloys. The use of Aluminum Strontium to modify the silicon phase of hypoeutectic aluminum silicon casting alloys from coarse platelets to a fine fibrous structure is a widely accepted practice. This results in improved casting soundness and mechanical properties, particularly ductility.Information provided by KB AlloysAl. Assoc. Registration No: H2019
Component Elements Properties Metric English Comments
Aluminum, Al 83.14 - 85.14 %
83.14 - 85.14 %
Barium, Ba 0.10 %
0.10 %
Calcium, Ca 0.050 %
0.050 %
Iron, Fe 0.30 %
0.30 %
Other, each 0.050 %
0.050 %
Other, total 0.15 %
0.15 %
Phosphorous, P 0.010 %
0.010 %
Silicon, Si 0.20 %
0.20 %
Strontium, Sr 14 - 16 %
14 - 16 %
Descriptive Properties Value Comments
Form Korrect Bar, Waffle Ingot, Buttons