Johnson Matthey JM No2S Soft Solder Flux

Category Metal , Nonferrous Metal , Solder/Braze Alloy
Manufacturer Johnson Matthey
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Johnson Matthey JM No2S Soft Solder Flux.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
A liquid non-corrosive flux for use on copper and brass. The residues are water soluble and non-corrosive, however it is recommended they are removed to prevent any possibility of contamination after soldering.Information provided by Johnson Matthey.
Thermal Properties Metric English Comments
Melting Point 150 - 300 °C
302 - 572 °F
Solidus 150 °C
302 °F
Liquidus 300 °C
572 °F