Ineos N12N-00 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos N12N-00 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Grade N12N-00 is a nucleated polypropylene impact copolymer with an excellent balance of stiffness and impact resistance for injection molding applications and compounding products used in Lawn and Garden applications. It has good stiffness and excellent impact resistance even at sub ambient temperature. This meets the requirements of U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Applications:General purpose injection moldingCompoundingLawn and Garden applicationsConsumer productsBenefits:Excellent impact to stiffness balanceLow temperature impact resistanceInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 72
72
ASTM D785
Tensile Strength, Yield 23.6 MPa
3430 psi
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Tensile Modulus 1.32 GPa
191 ksi
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
ASTM D790A
Izod Impact, Notched 1.01 J/cm
1.90 ft-lb/in
1/8" (3mm) notched bar; ASTM D256
NB
NB
1/8" (3mm) notched bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 92.3 °C
198 °F
ASTM D648
Optical Properties Metric English Comments
Gloss 64.5 %
64.5 %
60° angle; ASTM D523
Descriptive Properties Value Comments
Process Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution