Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos K44-15-123 HDPE Copolymer with Carbon Black

Category Polymer , Thermoplastic , Polyethylene (PE) , HDPE , High Density Polyethylene (HDPE), Carbon Black Filled
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms EXW, FOB, CFR, CIF
Payment Terms L/C, T/T, PayPal
Download PDF Ineos K44-15-123 HDPE Copolymer with Carbon Black.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Fortiflex® K44-15-123 is a black high density polyethylene copolymer designed specifically for extrusion of potable water, industrial, and mining pipe. It has NSF certification and is recognized by the Plastic Pipe Institute as having a PE 3408 rating. The natural version of this resin is available as Fortiflex® K44-15-122.2.5% Carbon Black Concentration
Physical Properties Metric English Comments
Density 0.955 g/cc
0.0345 lb/in³
ASTM D4883
Environmental Stress Crack Resistance >= 5000 hour
>= 5000 hour
Condition C; same value for Pipe Ring ESCR; ASTM D 1693
Melt Flow 13 g/10 min

@Load 2.16 kg,
Temperature 190 °C
13 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 68
68
ASTM D2240
Tensile Strength, Ultimate 31.0 MPa
4500 psi
ASTM D638
Tensile Strength, Yield 22.8 MPa
3310 psi
ASTM D638
Elongation at Break >= 800 %
>= 800 %
ASTM D638
Flexural Modulus 0.830 GPa
120 ksi
2% Secant-Method 1; ASTM D790
Izod Impact, Notched 3.20 J/cm
5.99 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Vicat Softening Point 126 °C
259 °F
ASTM D1525
Brittleness Temperature <= -118 °C
<= -180 °F
ASTM D746