Industeel NUCL 18.10 B4 Natural Boron (Min 1% wt) Alloyed 304 Stainless Steel

Category Metal , Ferrous Metal , Stainless Steel , T 300 Series Stainless Steel
Manufacturer Groupe Arcelor
Trade Name NUCL
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel NUCL 18.10 B4 Natural Boron (Min 1% wt) Alloyed 304 Stainless Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Isotope B10 has the property to capture neutrons produced by nuclear reactions. Natural boron contains about 19.9 at% or 18.45 wt % of B10 isotope, the remaining being B11 isotope. NUCL 18.10 B4 grade is a 304 stainless steel obtained by ingot casting and alloyed with 1 to 1,24 wt% natural boron additions. In order to avoid ferrite grain which reduce the ductility of the alloy, NUCL 18.10 B4 grade has been overalloyed in Nickel when compared to 304 grades. Molybdenum additions are sometimes considered to increase the corrosion resistance properties. The ingots rolled into plates are considered for nuclear applications (transport, casks, storage -in pools) of nuclear (waste) products. For specific purposes, some other grades are sometimes used. The boron content may thus be included in the 0.2-2 weight % range or/and alloys obtained by powder metallurgy (A type). CLI-FAFER can also produce 18-10 A or B type boron alloyed grades (included B10 enriched grades). Among the family of boron enriched 304 grades, NUCL 18-10 B4 grade is the most commonly used.Information provided by manufacturer.
Physical Properties Metric English Comments
Density 7.80 g/cc
0.282 lb/in³
Mechanical Properties Metric English Comments
Hardness, Brinell <= 217
<= 217
Typical
Hardness, Rockwell B <= 95
<= 95
Typical
Tensile Strength, Ultimate >= 515 MPa
>= 74700 psi
Minimum Guaranteed
610 MPa
88500 psi
Typical
Tensile Strength, Yield >= 210 MPa

@Strain 0.200 %
>= 30500 psi

@Strain 0.200 %
>= 225 MPa

@Strain 1.00 %
>= 32600 psi

@Strain 1.00 %
310 MPa

@Strain 0.200 %
45000 psi

@Strain 0.200 %
Typical
325 MPa

@Strain 1.00 %
47100 psi

@Strain 1.00 %
Typical
Elongation at Break >= 16 %
>= 16 %
19 %
19 %
Typical
Modulus of Elasticity 200 GPa
29000 ksi
Poissons Ratio 0.333
0.333
Calculated
Shear Modulus 75.0 GPa

@Temperature 20.0 °C
10900 ksi

@Temperature 68.0 °F
Thermal Properties Metric English Comments
CTE, linear 17.0 µm/m-°C

@Temperature 20.0 - 100 °C
9.44 µin/in-°F

@Temperature 68.0 - 212 °F
17.5 µm/m-°C

@Temperature 20.0 - 200 °C
9.72 µin/in-°F

@Temperature 68.0 - 392 °F
18.0 µm/m-°C

@Temperature 20.0 - 300 °C
10.0 µin/in-°F

@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.500 J/g-°C

@Temperature 20.0 °C
0.120 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 15.0 W/m-K

@Temperature 20.0 °C
104 BTU-in/hr-ft²-°F

@Temperature 68.0 °F
Component Elements Properties Metric English Comments
Boron, B 1.1 %
1.1 %
Carbon, C 0.013 %
0.013 %
Chromium, Cr 18.5 %
18.5 %
Iron, Fe 66.687 - 66.787 %
66.687 - 66.787 %
As remainder
Manganese, Mn 0.80 %
0.80 %
Nickel, Ni 12.5 %
12.5 %
Nitrogen, N <= 0.10 %
<= 0.10 %
Silicon, Si 0.30 %
0.30 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000950 ohm-cm

@Temperature 20.0 °C
0.0000950 ohm-cm

@Temperature 68.0 °F