Indium Corp. Indalloy 185 Cadmium Solder Alloy

Category Metal , Nonferrous Metal , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 185 Cadmium Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 8.73 g/cc
0.315 lb/in³
Thermal Properties Metric English Comments
Melting Point 340 - 395 °C
644 - 743 °F
Solidus 340 °C
644 °F
Liquidus 395 °C
743 °F
Component Elements Properties Metric English Comments
Cadmium, Cd 95 %
95 %
Silver, Ag 5.0 %
5.0 %