| Category | Metal , Nonferrous Metal , Precious Metal , Gold Alloy , Solder/Braze Alloy |
| Manufacturer | Indium Corporation of America |
| Trade Name | Indalloy |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Indium Corp. Indalloy 184 Gold Solder Alloy.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 15.4 g/cc | 0.556 lb/in³ |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 254.93 MPa | 36975 psi | |
| Modulus of Elasticity | 83.01 GPa | 12040 ksi | |
| Shear Strength | 220 MPa | 31900 psi |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 12.0 µm/m-°C @Temperature 20.0 °C |
6.67 µin/in-°F @Temperature 68.0 °F |
|
| Thermal Conductivity | 27.0 W/m-K @Temperature 85.0 °C |
187 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
| Melting Point | 363 °C | 685 °F | Eutectic |
| Solidus | 363 °C | 685 °F | |
| Liquidus | 363 °C | 685 °F |
| Component Elements Properties | Metric | English | Comments |
|---|---|---|---|
| Gold, Au | 96.8 % | 96.8 % | |
| Silicon, Si | 3.2 % | 3.2 % |