Imerys AMCâ„¢ 150 Ground Mica

Category Ceramic , Oxide , Aluminum Oxide , Silicon Oxide
Manufacturer Imerys (Kentucky-Tennessee Clay Co.)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Imerys AMCâ„¢ 150 Ground Mica.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
AMC 150 is a dry Ground Mica (complex potassium aluminum silicate) with a controlled particle size distribution. The inherent platy nature of AMC 150 enhances the release performance (anti-tack) in such rubber molding and sheet production.Information provided by Imerys
Physical Properties Metric English Comments
Specific Gravity 2.75 g/cc
2.75 g/cc
Bulk Density 0.352 g/cc
0.0127 lb/in³
Density 2.74 g/cc
0.0991 lb/in³
Brightness 80 %
80 %
Whiteness (Hunter L)
Particle Mesh Size 100 Mesh
100 Mesh
less than 0.8% retained
200 Mesh
200 Mesh
less than 21% retained
325 Mesh
325 Mesh
73% through; Alpine Air Jet Sieve
pH 7.9
7.9
Mechanical Properties Metric English Comments
Hardness, Mohs 2.5
2.5
Optical Properties Metric English Comments
Refractive Index 1.58
1.58
Processing Properties Metric English Comments
Moisture Content <= 0.30 %
<= 0.30 %