Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Pluracol® GP 730 Specialty Polyol

Category Fluid
Manufacturer BASF
Trade Name Pluracol®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Pluracol® GP 730 Specialty Polyol.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: Pluracol® GP polyols are a series of four trifunctional polyols formed by adding propylene oxide to a glycerine nucleus. All Pluracol GP polyols are used in the preparation of polyurethane coatings, elastomers, adhesives and sealants. Pluracol 1135i and 726 are also used in the preparation of flexible polyurethane foams.Information provided by BASF
Physical Properties Metric English Comments
Density 1.02 g/cc

@Temperature 48.9 °C
0.0368 lb/in³

@Temperature 120 °F
1.03 g/cc

@Temperature 37.8 °C
0.0372 lb/in³

@Temperature 100 °F
1.04 g/cc

@Temperature 25.0 °C
0.0376 lb/in³

@Temperature 77.0 °F
Viscosity 78 cP

@Temperature 48.9 °C
78 cP

@Temperature 120 °F
140 cP

@Temperature 37.8 °C
140 cP

@Temperature 100 °F
270 cP

@Temperature 25.0 °C
270 cP

@Temperature 77.0 °F
Molecular Weight 700 g/mol
700 g/mol
Thermal Properties Metric English Comments
Specific Heat Capacity 1.16 J/g-°C
0.277 BTU/lb-°F
Thermal Conductivity 0.125 W/m-K
0.868 BTU-in/hr-ft²-°F
Chemical Properties Metric English Comments
Total Acid Number <= 0.045
<= 0.045
STI 3063/3161
Processing Properties Metric English Comments
Moisture Content <= 0.050 %
<= 0.050 %
STI 3062
Descriptive Properties Value Comments
Composition Na & K
<10 ppm, STI 3038
Hydroxyl Number 222 - 237 mg KOH/g
STI 3007/3162
Users viewing this material also viewed the following: