Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ITW Plexus Plexusâ„¢ MA920 Methacrylate Adhesive

Category Polymer , Adhesive , Thermoset , Methacrylate , Methacrylate Adhesive
Manufacturer ITW Plexus
Trade Name Plexus™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ITW Plexus Plexusâ„¢ MA920 Methacrylate Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Two-part adhesive designed for structural bonding of thermoplastic, metal, and composite assemblies.All purpose, low odor, short open time.Information provided by Illinois Tool Works.
Physical Properties Metric English Comments
Density 0.971 g/cc
0.0351 lb/in³
Mixed
Viscosity 50000 - 70000 cP
50000 - 70000 cP
B
100000 - 125000 cP
100000 - 125000 cP
A
Mechanical Properties Metric English Comments
Tensile Strength at Break 18.6 - 20.7 MPa
2700 - 3000 psi
Elongation at Break 80 - 100 %
80 - 100 %
Tensile Modulus 0.517 - 0.689 GPa
75.0 - 100 ksi
Shear Strength 10.3 - 13.8 MPa
1500 - 2000 psi
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 121 °C
250 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Flash Point 10.6 °C
51.0 °F
TCC
Processing Properties Metric English Comments
Pot Life 4.0 - 6.0 min
4.0 - 6.0 min
Descriptive Properties Value Comments
Color Blue
Fixture Time 15-18 minutes
Gap Filling Max 0.375 in
Mix Ratio 10:1
By volume