ICO Polymers ICORENEâ„¢ 190-3561 LMDPE Rotational Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Linear Medium Density Polyethylene (LMDPE), Rotational Molded
Manufacturer ICO Polymers (A Schulman Inc.)
Trade Name ICORENE™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ICO Polymers ICORENEâ„¢ 190-3561 LMDPE Rotational Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Description: ICORENE 190-1332 is a linear medium density polyethylene copolymer developed for rotational molding. It has a good balance of properties such as toughness, easy flow and stiffness. Key Characteristics: good physical properties, easy molding, controlled release. Applications: This ICORENE® grade is particularly sutiable for use in general purpose applications. Information provided by ICO Polymers.A Schulman acquired ICO, Inc. in 2010.
Physical Properties Metric English Comments
Density 0.934 g/cc
0.0337 lb/in³
ASTM D1505
ESCR 10% Igepal® 100 hour
100 hour
F50; ASTM D1693
Melt Index of Compound 6.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 55
55
ASTM D2240
Tensile Strength, Yield 18.0 MPa
2610 psi
50 mm/min; ASTM D638
Elongation at Break 500 %
500 %
50 mm/min; ASTM D638
Flexural Modulus 0.700 GPa
102 ksi
1.3 mm/min; ASTM D790
Impact 21

@Temperature -20.0 °C
21

@Temperature -4.00 °F
J/mm, instrumented impact, rotomolded test sample; ICO R&D1.14
Descriptive Properties Value Comments
UV Light Weatherometer Test 8000 hours
ASTM G26