Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Huntsman HY 815 US Polyamide

Category Polymer , Thermoset , Epoxy
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman HY 815 US Polyamide.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Approx. H+ equivalent weight 150. Mix Ratio with GY 6010 is 81.Comments/Applications: Solvent free, high molecular weight, low amine content. Superior adhesion, easily pigmented. Trade sale paint enamels. Industrial maintenance, FDA. Flexible mix ratio. Usually used with "Type 1" epoxy resins.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 50000 - 75000 cP
50000 - 75000 cP
Processing Properties Metric English Comments
Pot Life 600 min
600 min
Users viewing this material also viewed the following: